MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LG Chemical IP-20
Categories: Fluid

Material Notes: Structure & Characteristics: C5H10. A ring-structured saturated hydrocarbon. Present in naphtha pyrolysis oil and is obtained by distillation followed by isolation of n-pentane extraction remnants or C5 products.

Uses: As a polyurethane foaming agent, it is increasingly used in place of Freon foaming agent.

CAS: 78-78-4 and 109-66-0

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.620 g/ccn-Pentane
 0.620 g/ccIso-Pentane
Volatiles 100 %n-Pentane
 100 %Iso-Pentane
Vapor Pressure 426 torr
@Temperature 20.0 °C
Vapor Density=2.48, n-Pentane
 595 torr
@Temperature 20.0 °C
Vapor Density=2.48, Iso-Pentane
 
Thermal PropertiesOriginal ValueComments
Melting Point -160.5 °CIso-Pentane
 -130.5 °Cn-Pentane
Boiling Point 28.0 °CIso-Pentane
 36.0 °Cn-Pentane
Flash Point <= -49.0 °C
Ignition Temperature 260 °CAutoignition
 
Descriptive Properties
ComponentsCYCLO-PENTANE<1%
 cyclo-Pentane<1.0%
 higher than n-Pentane<0.2%
 Isopentane18-22%
 ISO-PENTANE18-22%
 low than iso-Pentane<0.5%
 LOWER THAN ISO-PENTANE<0.5%
 n-Pentane68-76%
 total olefin<400 ppm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLAY763 / 148773

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.