MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives Circalok™ 6404 A/B Two Component Encapsulant
Categories: Polymer; Thermoset

Material Notes: Circalok™ 6404 A/B encapsulant is a general purpose, encapsulating material for any application where a fast cure, mechanical shock resistant system is required.

Features: Low Viscosity, Excellent Hydrolytic Stability - resists moisture and protects components. Contains no MOCA or TDI

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/cc
@Temperature 25.0 °C
Viscosity 900 cP
@Temperature 25.0 °C
mixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80
Tensile Strength 1935 psi
@Temperature 25.0 °C
cured
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cm
@Temperature 25.0 °C
cured
Dielectric Constant 3.6
@Frequency 1000 Hz,
Temperature 25.0 °C
cured
Dielectric Strength 600 V/mil
Dissipation Factor 0.14
@Frequency 1000 Hz,
Temperature 25.0 °C
cured
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °C
Minimum Service Temperature, Air -50.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.08333 - 0.1666 hour
@Temperature 100 °C
 0.500 - 0.750 hour
@Temperature 25.0 °C
 48.0 - 72.0 hour
@Temperature 25.0 °C
post cure
Pot Life 5.00 min
@Temperature 25.0 °C
Shelf Life 6.00 Monthin closed containers
 
Descriptive Properties
AppearanceAmber LiquidMixed
Mix Ratio22 to 10R to I, by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9266 / 232622

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.