MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Syncure™ System S100NA Polyethylene, Crosslinked (XLPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Syncure™ systems are two part moisture crosslinkable compounds, UL bulletinized easy processing, high strength, colorable cable insulation compound suitable for service entrance cables. RoHS compliant.

NOTE: Typical Properties measured on 14 AWG with 30 mil wall. STORAGE AND HANDLING: Use within 48 hours once package is open to avoid self-curing and scrap.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.923 g/ccASTM D792
Deformation 10 %
@Temperature 131 °C,
Time 3600 sec
500 g; UL 1581
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 4610 sec; ASTM D2240
 52ASTM D2240
Tensile Strength, Yield 19.3 MPaType IV, 510 mm/min; ASTM D638
Elongation at Break 400 %Type IV, 510 mm/min; ASTM D638
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.14ASTM D150
Dielectric Strength 39.0 kV/mmASTM D149
Dissipation Factor 0.0020ASTM D150
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 90.0 °CUL Temperature Rating
 
Component Elements PropertiesOriginal ValueComments
Sulfate, SO4 <= 0.020 %
 
Descriptive Properties
Agency RatingsMIL C-24643
 UL 854
AppearanceNatural Color
Catalyst Masterbatch5%S-1010B
FormsPellets
Gel Content72%ASTM D2765; Crosslinked PE, Method B (NonReferee Test)
Generic MaterialXLPE
Generic NamePolyethylene, Crosslinked (XLPE)
Grafted Base Resin95%S-1054A
Processing MethodExtrusion Coating
Regional AvailabilityNorth America
Retention of Tensile Elongation85%158°C, 1.91 mm; 168 hr, UL Standard
 90%121°C, 1.91 mm; 336 hr, UL Standard
Retention of Tensile Strength90%158°C, 1.91 mm; 168 hr, UL Standard
 95%121°C, 1.91 mm; 336 hr, UL Standard
UsesWire & Cable Applications
Wire TypesUSE
 USE-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Polidan® EC/110 Polyethylene, Crosslinked (XLPE)
Overview of materials for Polyimide
Overview of materials for Nylon 6, 40% Glass Fiber Filled
Inhance Fluoro-Seal INHANCE® UH-1080 Ultra High Molecular Weight Polyethylene
Graft Polymer GRAFTABOND™ UH-SAN 00055 PDIM Ultra High Molecular Weight Polyethylene, grafted with Styrene Acrylonitrile

PH0POL0321 / 144890

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.