MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Celanese FORTRON 1200L1 PPS, Specialty
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Fortron 1200L1 is an unfilled grade recommended primarily for extrusion applications. It has a high melt viscosity and tensile elongation. Recommended processing conditions are similar to those of our standard unfilled PPS grades.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.34 g/ccISO 1183
Water Absorption at Saturation 0.020 %ISO 62
Viscosity 430000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 93ISO 2039-2
Tensile Strength at Break 88.0 MPa50mm/min; ISO 527-2/1A
Elongation at Break 15 %50mm/min; ISO 527-2/1A
Elongation at Yield 3.0 %50mm/min; ISO 527-2/1A
Tensile Modulus 4000 MPa50mm/min; ISO 527-2/1A
Flexural Strength 141 MPaISO 178
Flexural Modulus 4100 MPaISO 178
Charpy Impact Unnotched 200 kJ/m²ISO 179/1eU
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.0
@Frequency 10000 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 30.0 kV/mmIEC 60243-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 40.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 42.0 µm/m-°CISO 11359-2
Melting Point 275 °C10°C/min; ISO 11357-1,-2,-3
Glass Transition Temp, Tg 90.0 °CISO 11357-1,-2,-3
 
Processing PropertiesOriginal ValueComments
Drying Temperature 110 - 120 °C
Dry Time 3.00 - 4.00 hour
Moisture Content <= 0.020 %
 
Descriptive Properties
Injection moldingYes
Sheet extrusionYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese FORTRON 317 PPS, Unfilled
Celanese FORTRON 1120L4 PPS, 20% Specialty
Celanese FORTRON 1140L0 PPS, 40% Glass Reinforced
Celanese FORTRON 1342L4 PPS, 40% Specialty
Celanese FORTRON 214 PPS, Unfilled

PHCQ275 / 178730

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.