MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PTS PBT-101G0 PBT Resin
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Typical Applications: Appliance parts

Information provided by PTS LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D792
Moisture Absorption at Equilibrium 0.10 %50% RH; ASTM D570
Linear Mold Shrinkage, Flow 0.020 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.014 cm/cmASTM D955
Melt Flow 26 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 52.0 MPaASTM D638
Elongation at Break >= 100 %ASTM D638
Tensile Modulus 2600 MPaASTM D638
Flexural Strength 80.0 MPaASTM D790
Flexural Modulus 2500 MPaASTM D790
Izod Impact, Notched (ISO) 5.40 kJ/m²ASTM D256
Izod Impact, Unnotched (ISO) 80.0 kJ/m²ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 145 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °CASTM D648
Flammability, UL94 HB
@Thickness 0.380 mm
 HB
@Thickness 0.800 mm
 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PTS PBT-1090 PBT Resin
PTS PCA-3013 High Flow PC/PBT Alloy
PTS PCA-3015 Low Temperature Impact PC/PBT Alloy
PTS PBT-1100 PBT Resin
A. Schulman VOLOY™ 462 Hybrid Reinforced PBT Alloy

PZ9PU921 / 135378

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.