MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese Zytel® 101L BKB080 PA66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Unreinforced Polyamide 66

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³DAM; ISO 1183
Water Absorption 1.2 %
@Thickness 3.00 mm,
Time 86400 sec
1.2 %
@Thickness 0.118 in,
Time 24.0 hour
Immersion; DAM; Sim. to ISO 62
Viscosity Number 145 cm³/g1.45 dl/gDAM; ISO 307, 1157, 1628
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 595950% RH; ISO 2039-2
 7979DAM; ISO 2039-2
Hardness, Rockwell R 10810850% RH; ISO 2039-2
 121121DAM; ISO 2039-2
Ball Indentation Hardness 85.0 MPa12300 psiH 358/30; DS; 50% RH; ISO 2039-1
 160 MPa23200 psiH 961/30; DAM; ISO 2039-1
 180 MPa26100 psiH 358/30; DS; DAM; ISO 2039-1
Tensile Strength, Yield 55.0 MPa7980 psi50% RH; ISO 527-1/-2
 82.0 MPa11900 psiDAM; ISO 527-1/-2
Elongation at Break 25 %25 %Nominal; DAM; ISO 527-1/-2
 >= 50 %>= 50 %Nominal; 50% RH; ISO 527-1/-2
Elongation at Yield 4.3 %4.3 %DAM; ISO 527-1/-2
 25 %25 %50% RH; ISO 527-1/-2
Tensile Modulus 1.40 GPa203 ksi50% RH; ISO 527-1/-2
 3.10 GPa450 ksiDAM; ISO 527-1/-2
Flexural Strength 54.0 MPa7830 psi50% RH; ISO 178
 90.0 MPa13100 psiDAM; ISO 178
Flexural Modulus 2.80 GPa406 ksiDAM; ISO 178
Poissons Ratio 0.370.37DAM
 0.430.4350% RH
Izod Impact, Notched (ISO)  4.00 kJ/m²
@Temperature -40.0 °C
1.90 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 180/1A
 4.00 kJ/m²
@Temperature -40.0 °C
1.90 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 5.50 kJ/m²
@Temperature 23.0 °C
2.62 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 180/1U
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 0.450 J/cm²
@Temperature -30.0 °C
2.14 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.550 J/cm²
@Temperature 23.0 °C
2.62 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 475 V475 VCTI M; DAM; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.68 J/g-°C0.402 BTU/lb-°FSolid
Thermal Conductivity 0.240 W/m-K1.67 BTU-in/hr-ft²-°FSolid
Melting Point 262 °C504 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 190 °C374 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FDAM; ISO 75-1/-2
Glass Transition Temp, Tg 40.0 °C104 °F10°C/min; 50% RH; ISO 11357-1/-2
 70.0 °C158 °F10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94  V-2
@Thickness 0.710 mm
V-2
@Thickness 0.0280 in
DAM; IEC 60695-11-10
 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
DAM; IEC 60695-11-10
Glow Wire Ignition Temperature  725 °C
@Thickness 0.750 mm
1340 °F
@Thickness 0.0295 in
DAM; IEC 60695-2-13
 750 °C
@Thickness 1.50 mm
1380 °F
@Thickness 0.0591 in
DAM; IEC 60695-2-13
 800 °C
@Thickness 3.00 mm
1470 °F
@Thickness 0.118 in
DAM; IEC 60695-2-13
 
Processing PropertiesMetricEnglishComments
Melt Temperature 275 - 290 °C527 - 554 °FRange, Extrusion
 285 °C545 °FOptimum, Extrusion
 290 °C554 °FOptimum, Injection
 280 - 300 °C536 - 572 °FRange, Injection
Mold Temperature 70.0 °C158 °FOptimum, Injection
 50.0 - 90.0 °C122 - 194 °FInjection
Ejection Temperature 190 °C374 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
 4.00 - 6.00 hour4.00 - 6.00 hourExtrusion, Dehumidified Dryer
Moisture Content <= 0.20 %<= 0.20 %Injection
Hold Pressure 50.0 - 100 MPa7250 - 14500 psiRange, Injection
 
Descriptive Properties
Drying RecommendedyesInjection
Emission of organic compounds (µgC/g)38VDA 277
FMVSS ClassDNIISO 3795 (FMVSS 302)
Fogging (%)99F-value (refraction); ISO 6452; DAM
Fogging (mg)0.1G-value (condensate); ISO 6452; DAM
ISO designationISO 16396-PA66,,M1CG1R,S14-030
Max. screw tangential speed (m/s)0.4Injection
Odor Class3VDA 270
Part Marking Code>PA66<ISO 11469
PolymerPA66
Processing Hold Pressure Time (s/mm)4Injection
Resin IdentificationPA66ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® 101L BKB009 PA66
Celanese Zytel® 101L NC010 PA66
Celanese Zytel® 101 NC010 PA66
Celanese Zytel® 101F NC010 PA66
Celanese Zytel® 103FHSA NC010 PA66

PDSX5296 / 197936

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.