MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik SOLIMIDE® AC-530 Polyimide Foam
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: SOLIMIDE AC-530 foam is utilized in aircraft, aerospace, and industrial markets as a lightweight, non-wicking, fire resistant, thermal and acoustic insulation material. SOLIMIDE AC-530 foam is used in a variety of applications, including expansion/contraction joints in cryogenic applications, as well as aircraft fuselage, under floor, and duct insulation. SOLIMIDE AC-530 foam is compatible with many different facings, coatings and adhesives. It can be cut into numerous shapes or sizes to meet end use requirements.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.00560 g/ccASTM D3574
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 0.00276 MPa25% Compression; ASTM D3574
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0490 W/m-KASTM C518
Maximum Service Temperature, Air 200 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik SOLIMIDE® Densified HT Foam
Evonik SOLIMIDE® AC-550 Polyimide Foam
Evonik SOLIMIDE® HT 340 Polyamide Foam
Braskem Evateno® 3019 PE EVA Foam Copolymer
DuPont Mobility and Materials Vespel® SF-0920 Polyimide Foam, Low Density

PEVONIL660 / 196864

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.