MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Zyvex Performance Materials Aroply™ 350 Nano-Engineered Composite Film Adhesive
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite

Material Notes: Aroply™ 350 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported carrier. Cured adhesive characteristics are designated by exceptionally high shear and peel strengths on a variety of substrates at temperatures up to 350F. This film adhesive is designed for both solid panel and honeycomb constructions. Aroply™ 350 contains an optimum level of carbon nanotubes for additional toughness and enhanced mechanical properties. The carbon nanotubes use molecular dispersion technology to ensure enhancements are evenly distributed throughout the adhesive.

Features:

  • Semi-tacky for adherence to desired location
  • Long Open Time: 30 days in standard shop conditions
  • Adaptable to many processes

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 1000 cP
@Temperature 120 °C
Rheology, 2°C/min
 1100 cP
@Temperature 160 °C
Rheology, 2°C/min
 8000 cP
@Temperature 80.0 °C
Rheology, 2°C/min
 800000 cP
@Temperature 40.0 °C
Rheology, 2°C/min
 1.10e+7 cP
@Temperature 175 °C
Rheology, 2°C/min
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1000 psiFlatwise, 90 min @ 350°F, Spring Clamp Pressure, Abraded 6061-T6 Untreated; ASTM C297M
Shear Strength 1500 psi
@Temperature 177 °C
2 hr soak, 90 min @ 350°F, Spring Clamp Pressure, FPL Acid Etched 6061-T6; ASTM D1002
 3000 psi
@Temperature 177 °C
90 min @ 350°F, Spring Clamp Pressure, FPL Acid Etched 6061-T6; ASTM D1002
 3800 psi
@Temperature 121 °C
90 min @ 350°F, Spring Clamp Pressure, FPL Acid Etched 6061-T6; ASTM D1002
 4200 psi
@Temperature 21.1 °C
90 min @ 350°F, Spring Clamp Pressure, FPL Acid Etched 6061-T6; ASTM D1002
Peel Strength 17.0 pli
@Temperature 21.1 °C
T-Peel, 90 min @ 350°F, Spring Clamp Pressure, FPL Acid Etched 6061-T6; ASTM D1876
 26.0 pli
@Temperature 121 °C
T-Peel, 90 min @ 350°F, Spring Clamp Pressure, FPL Acid Etched 6061-T6; ASTM D1876
 32.0 pli
@Temperature 177 °C
Roller Peel, 90 min @ 350°F, Spring Clamp Pressure, FPL Acid Etched 6061-T6; ASTM D3167
 37.0 pli
@Temperature 21.1 °C
Roller Peel, 90 min @ 350°F, Spring Clamp Pressure, FPL Acid Etched 6061-T6; ASTM D3167
 43.0 pli
@Temperature 121 °C
Roller Peel, 90 min @ 350°F, Spring Clamp Pressure, FPL Acid Etched 6061-T6; ASTM D3167
 
Descriptive Properties
Drum Peel19.8 in-lb/inTool Side Up, 2 hrs @ 250°F, 30 psi, 6061 T6 Abraded, 1” Nomex 3 lb core 1/8” cell
 20.5 in-lb/inTool Side Down, 2 hrs @ 250°F, 30 psi, 6061 T6 Abraded, 1” Nomex 3 lb core 1/8” cell
Load to Failure606 lbf5 lb Core, 6 hrs @ 220°F, Vacuum Bag
 669 lbf8 lb Core, 6 hrs @ 220°F, Vacuum Bag

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Hysol EA 9658 Film Adhesive
Zyvex Performance Materials Aroply™ 250 Nano-Engineered Composite Film Adhesive
Zyvex Performance Materials Arovex™ 250 Carbon Nanotube Strengthened Prepreg
Zyvex Performance Materials Arovex™ HT 250 Nano-Engineered Composite Prepreg System
Garlock 9800 Compressed Carbon Fiber Gasketing, SBR Binder

PZYVEX91D / 159343

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.