Hostacom ERC 161N is a 16% talc filled PP copolymer, with excellent flowability, good stiffness and good scratch resistance. This grade is delivered in customer customized colors, some properties may be slightly altered upon color selected. Applications: Interior Trims.Information provided by LyondellBasell. |