MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

BEC Materials SEBS 507
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: Thermoplastic elastomer SEBS (styrene ethylene butylene styrene) block copolymer 507 is a special material for the preparation of high value-added self-adhesive protective film, as a two-layer or multi-layer co-extruded film (mostly PE film) in the adhesive layer. The purpose is to prevent the surface of the protected substrate from being damaged or contaminated during transportation, assembly or processing. Compared with the traditional type of protective film, self-adhesive protective film with low cost, no residual plastic images, uniform viscosity and easy to control, etc., and there is no recovery or solvent residues and other problems.

Application: Self-adhesive protective film

Information provided by BEC Materials, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.20 %<= 0.20 %
 
Chemical PropertiesMetricEnglishComments
Styrene Content 15 %15 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5656
Tensile Strength >= 12.4 MPa>= 1800 psi
Elongation at Break >= 874 %>= 874 %
300% Modulus >= 2.10 MPa>= 305 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBECM079 / 307032

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.