Notes: Elexar EL-2934N is a high performance UL V-0 flame retardant thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. Elexar EL-2934N is a high hardness, high density, low flow grade that is UV stabilized and RoHS compliant. This UL listed grade is easily colorable and is suitable for both injection molding and extrusion. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Brominated; Flame Retardant; General Purpose; Good Colorability; Halogenated; Heat Aging Resistant; High Density; High Elongation; High Hardness; High Specific Gravity; High Tensile Strength; Low Flow; Sunlight Resistant (720 hours); UV Resistant Uses: Appliance Wire Insulation; Appliance Wire Jacketing. Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Ribbons; Rubber Replacement; Terminal Cable Jacketing; Underground Power Cable; Wire & Cable Applications; Wire Jacketing RoHS Compliance: RoHS Compliant UL File Number: QMFZ2. E54709 Form: Pellets Processing Method: Injection Molding; Extrusion Information provided by Teknor Apex |