MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ LUBRICOMP™ Compound MG004 Polypropylene, Unspecified (PP, Unspecified)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: LNP LUBRICOMP MG004 compound is based on Polypropylene (PP) resin containing graphite powder. Added features of this grade include: Wear Resistant.

Features: Wear resistant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.011 - 0.016 cm/cm0.011 - 0.016 in/inSABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 33.0 MPa4790 psi5 mm/min; ISO 527
Elongation at Yield 4.4 %4.4 %5 mm/min; ISO 527
Tensile Modulus 2.70 GPa392 ksi1 mm/min; ISO 527
Flexural Strength 54.0 MPa7830 psiyield, 2 mm/min; ISO 178
Flexural Modulus 2.90 GPa421 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²9.52 ft-lb/in²80*10*4; ISO 180/1U
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 92.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
51.1 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 129 µm/m-°C
@Temperature 23.0 - 60.0 °C
71.7 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 122 °C252 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C160 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 
Processing PropertiesMetricEnglishComments
Zone 2 215 - 225 °C419 - 437 °F
Zone 3 240 - 250 °C464 - 482 °F
Melt Temperature 225 - 250 °C437 - 482 °FInjection Molding
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80895 / 288842

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.