MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) RHODOLINEĀ® 3100 Surfactant
Categories: Fluid

Material Notes: Standard Applications: RHODOLINEĀ® 3100 is an excellent APE-free non-ionic wetting/dispersing agent for use in waterborne paint formulations: low to medium HLB organic pigment wetting including carbon black and lampblack and substrate wetting; replaces APE wetting agents within HLB range of 11-13. Recommended usage levels typically are 0.1-0.5% as wetting agents for paint formulations, 1-2% based on pigment wetting and 5-15% on the pigment weight for pigment preparation.

Chemical Name: Nonionic Wetting and Dispersing Agent

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 - 1.15 g/ccRP-17617
Solids Content 84 - 86 %CEM, 30% Power; RP-0540
Viscosity <= 3000 cP#4 sp @ 60 rpm; RP-0659
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceLight yellow to amber liquidRP-0064

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOLVAY799 / 218527

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.