MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Abatron WoodEpox® Wood Replacement Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: WoodEpox® is a shrink-free adhesive putty wood replacement compound that can be used in any thickness in structural and decorative applications to replace, repair, extend, or fill wood and materials. WoodEpox® is ideal for repairing, replacing, or adding to wood and most rigid surfaces, as well as to dried out, rotted, or spongy wood consolidated with LiquidWood®. It can be used on windowsills, thresholds, window and door frames, columns, stair steps, balustrades, floors, capitals, moldings, doors, shutters, indoor and outdoor furniture, statues, archaeological and art restoration. WoodEpox® bonds permanently with high strength to most surfaces. It fills cracks, holes, and voids of any size without the shrinking and crumbling of common wood fillers. It can replace or add missing or new sections in window frames and sills, furniture, sculptures, structural and decorative components, indoors and outdoors. Because of its strength and durability, it can be a permanent solution. WoodEpox® succeeds because it can be painted, stained, wood-grained, sawed, nailed, planed, sanded, carved, and machined like wood. It can be cast into shapes and sculpted by hand before hardening. It can also be carved after hardening. It bonds equally well to ceramics, concrete, metal, glass, fiberglass, and most rigid surfaces. It contains no VOC's or noxious odors. It has a light, neutral color than can be changed, while mixing with stains, dyes, or pigments. It has a no slump paste consistency that allows it to be applied like a putty to fill gaps, holes, or to build-up virtually any thickness and shape. Contents ? WoodEpox® is a light-weight epoxy adhesive system consisting of 2 components: resin paste (A) and hardener paste (B). When A and B are mixed in equal volumes, the blend hardens within 1-2 hours into a light-weight, non-shrinking, tough adhesive mass with high dimensional stability, chemical, water, heat, and weather resistance. 100% solids. 1/1 ratio. 20 minute pot life.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
Volatile Organic Compounds (VOC) Content 0.00 g/l
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 53 - 55
Tensile Strength at Break 2500 psi
Elongation at Break 4.0 %
Compressive Strength 2300 - 2800 psi
 
Processing PropertiesOriginal ValueComments
Pot Life 20 min
 
Descriptive Properties
Hardening Time (min)60-120

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Abatron LiquidWood® Deep Penetrating Wood Consolidant
European White Oak Wood
European Ash Wood
Epoxy Technology EPO-TEK® T7109 Thermally Conductive Epoxy
Old Hickory UltraCast Slurry PC-2000 Kentucky Ball Clay

PABC884 / 107868

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.