MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
GEHR Plastics Ultem® 2300 PEI-30 GF, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), 30% Glass Fiber

Material Notes: Polyetherimide has high mechanical strength in combination with a good chemical and heat resistance, and good dimensional stability. Its unique torque strength permits the economical substitution of machined fabricated small parts from steel. Main Characteristics: higher thermal properties; excellent dimensional stability; much higher stiffness

Information provided by GEHR Plastics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.51 g/ccASTM D792
Moisture Absorption at Equilibrium 0.16 %50% RH; ASTM D570
Water Absorption at Saturation 0.90 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 23000 psiASTM D638
Tensile Strength, Yield 24500 psiASTM D638
Elongation at Break 3.0 %ASTM D638
Modulus of Elasticity 1350 ksiASTM D638
Flexural Strength 33000 psiASTM D638
Izod Impact, Notched 1.60 ft-lb/inASTM D256
Izod Impact, Unnotched 8.00 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmASTM D257
Surface Resistance 1.00e+13 ohm
Dielectric Constant 3.7
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 33.0 kV/mmASTM D149
Dielectric Loss Index 0.0015
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 µin/in-°FASTM D696
Thermal Conductivity 1.50 BTU-in/hr-ft²-°F
@Temperature 20.0 °C
ASTM C177
Melting Point 410 °FASTM D3418
Maximum Service Temperature, Air 340 °FUL 746B
Deflection Temperature at 0.46 MPa (66 psi) 414 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 410 °FASTM D648
Vicat Softening Point 442 °FVST/B/50; ASTM D1525
Minimum Service Temperature, Air -58.0 °FUL 746B
Glass Transition Temp, Tg 410 °FASTM D 3418
Flammability, UL94 V-0
 
Compliance PropertiesOriginal ValueComments
FDA NoPhysiological indifference
 
Descriptive Properties
Acid ResistanceYes
Aromatic ResistanceYes
Bondabilityyes
CKW ResistanceLimited
Hydrocarbonate ResistanceYes
Hydroxide ResistanceYes
Ketone ResistanceNo
Physiological indifferenceNSF, 51
Resistance to Hot WaterYes
UV Stabilizationyes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quantum PEI - Ultem® 30% Glass Fiber Filled
Ensinger TECAPEI® 30% Glass Reinforced, made from Ultem® 2300 PEI
Overview of materials for Polycarbonate, 20% Glass Filled
Mitsubishi Novaduran® 5810G30 Polybutylene Terephthalate
Professional Plastics Ultem Polyetherimide Film

PGEHR055 / 122038

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.