MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Dow Dowlex™ 2045.11S PE
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description:
  • For high speed, thin film applications
  • Additional thermal stability
  • Complies with US FDA 21 CRF 177.1520©3.2a
  • Complies with Canadian HPFB No Objection (with Limitations)
  • Complies EU, No 10/2011
  • Consult the regulations for complete details

Availability: Asia Pacific; Latin America; North America

Additive: Antiblock: 3000 ppm; Processing Aid: No; Slip: 1200 ppm

Agency Ratings: EU, No 10/2011; FDA 21 CRF 177.1520©3.2a; Canadian HPFB No Objection

Form: Pellets

Processing Method: Blown Film

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ASTM D792
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 3000 ppm3000 ppm
Slip Level 1200 ppm1200 ppm
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance 31.1 N7.00 lb (f)
Film Tensile Strength at Yield, MD 13.4 MPa1940 psiASTM D882
Film Tensile Strength at Yield, TD 14.1 MPa2050 psiASTM D882
Film Elongation at Break, MD 540 %540 %ASTM D882
Film Elongation at Break, TD 660 %660 %ASTM D882
1% Secant Modulus 211 MPa30600 psiMD; ASTM D882
 234 MPa33900 psiTD; ASTM D882
2% Secant Modulus 0.172 GPa24.9 ksiMD; ASTM D882
 0.189 GPa27.4 ksiTD; ASTM D882
Puncture Energy 1.24 J0.917 ft-lb
Elmendorf Tear Strength MD 440 g440 gASTM D1922
Elmendorf Tear Strength TD 630 g630 gASTM D1922
Dart Drop Test 180 g0.397 lbASTM D1709A
Film Tensile Strength at Break, MD 46.1 MPa6690 psiASTM D882
Film Tensile Strength at Break, TD 35.3 MPa5120 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 122 °C252 °F
Vicat Softening Point 104 °C219 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 20 %20 %ASTM D1003
Gloss 34 %34 %45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 216 °C420 °FExtrusion
Blow-up Ratio (BUR) 2.52.5
 
Descriptive Properties
Film Puncture Resistance75 ft-lb/in3
Film Toughness1330 ft-lb/in3MD, ASTM D882
 1370 ft-lb/in3TD, ASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF412 / 311105

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.