MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LyondellBasell Hostalen ACP 5231 D High Density Polyethylene (HDPE), Blow Molding Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Hostalen ACP 5231 D is a high density polyethylene resin used in small blow molding applications such as packaging, consumer goods and toys. It exhibits a very good combination of high stress cracking resistance, stiffness and good chemical resistance. Hostalen ACP 5231 D is delivered in pellet form, demonstrates good organoleptic properties, contains antioxidants and has a broad molecular weight distribution. Applications: Bottles For Consumer Goods, Bottles for Industrial Use, Jerry Cans, Sports, Leisure & Toys

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 31.2 lb/ft³
Density 0.952 g/ccISO 1183-1
Environmental Stress Crack Resistance >= 1200 hour
@Temperature 80.0 °C
Cond. B, 10% Arkopal N100; ASTM D1693
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
 1.2 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133-1
 22 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62ISO 868
Ball Indentation Hardness 51.0 MPaISO 2039-1
Tensile Strength, Yield 25.0 MPaISO 527-1,-2
Elongation at Yield 8.0 %ISO 527-1,-2
Tensile Modulus 1100 MPaISO 527-1,-2
Charpy Impact Unnotched 6.00 kJ/m²
@Temperature -30.0 °C
Type 1, Edgewise, Notch A; ISO 179
Tensile Impact Strength 75.0 kJ/m²
@Temperature -30.0 °C
notched; ISO 8256
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 210 °C
 
Descriptive Properties
FNCT (hrs)30ISO 16770, 3.5 MPa, 2% Arkopal, N100, 80°C
Processing MethodExtrusion blow molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
Arkema Solarkote® H300 Acrylic

PEQT8447 / 220082

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.