MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ASI® Pipe Sealer Torque 181 Anaerobic Urethane Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: Torque 181 is a high strength anaerobic adhesive for locking and sealing thread connections. Highly resistant to heat, corrosion, vibrations, water, gases, oils, hydrocarbons and many chemicals. Maintains unaffected curing properties up to 200 °C on any metal surface.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc
@Temperature 25.0 °C
1.10 g/cc
@Temperature 77.0 °F
uncured
Brookfield Viscosity 3500 cP
@Temperature 25.0 °C
3500 cP
@Temperature 77.0 °F
Uncured. Spindle 4- 2.5 rpm
Storage Temperature 8.00 - 28.0 °C46.4 - 82.4 °Funcured
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 0.117 - 0.255 MPa17.0 - 37.0 psi24 hrs 20° on steel; ISO 10123
 0.138 - 0.241 MPa20.0 - 35.0 psi24 hrs 20° on steel; DIN 54452
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°F@ 20° on steel 24 hrs; ASTM D696
Specific Heat Capacity 0.300 J/g-°C0.0717 BTU/lb-°F20° on steel 24 hours. Cured
Thermal Conductivity 0.100 W/m-K
@Time 86400 sec
0.694 BTU-in/hr-ft²-°F
@Time 24.0 hour
Cured. 20° on steel; ASTM C177
Maximum Service Temperature, Air 200 °C392 °F20°C on steel 24 hrs.
Minimum Service Temperature, Air -55.0 °C-67.0 °F20°C on steel 24 hrs.
Flash Point >= 100 °C>= 212 °Funcured
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 20.0 °C
12.0 Month
@Temperature 68.0 °F
uncured
 
Descriptive Properties
Chemical ClassUrethane Methacrylate
Color / appearanceGreen, fluorescent liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASINC9193 / 233559

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.