AFLAS® MZ is a terpolymer composed of tetrafluoroethylene, propylene and vinylidene fluoride. AFLAS® MZ offers a good balance of chemical resistance and improved low temperature performance and is categorized in ASTM D 1418-01 as class FKM, type four. Information provided by Asahi Glass Company, Inc. |