MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Reynolds duoMatrix™ -G Polymer additive system
Categories: Other Engineering Material

Material Notes: Product Overview: duoMatrix™-G is a new three component polymer additive system that greatly enhances the physical properties of alpha gypsum products duoMatrix™-G (Matrix-G™ for short) reduces the demold and drying time of gypsum and drastically reduces water permeability making it suitable for both interior and exterior applications (for exterior use, product must be sealed – see “post finishing” section). Matrix™-G has less odor and yields elements that are a brighter white than competing products. Matrix™-G is easy to use and can be cast solid, laid up by hand with chopped fiber or sprayed. Fully cured pieces can be painted, sanded, machined and polished. Matrix™-G is used to make lightweight pieces that are very strong and water-resistant. Applications include making architectural elements, reproducing sculpture and special effects. Vibrant colors are possible by adding pigments. Metal powders (bronze, pewter, brass, etc.) can be added to give the look of real metal castings at a fraction of the cost. You can duplicate the look of marble or ceramic by adding inexpensive fillers. When used with United States FGR 95 Alpha Gypsum, Matrix™-G has received a flame rating of UL-94V-O and meets ASTM E-84, Class A (or 1) flame rating for building materials, which means this product meets the highest standards for both flame and smoke.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.584 g/cc1.584 g/cc
Water Absorption 0.25 %0.25 %after 24 hour water soak
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 22.8 - 37.9 MPa3300 - 5500 psi
Flexural Strength 51.7 - 67.6 MPa7500 - 9800 psi
Compressive Strength 44.8 - 65.5 MPa6500 - 9500 psi
Tensile Impact Strength 367 kJ/m²175 ft-lb/in²
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.0 °C199 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 90.0 - 120 min1.50 - 2.00 hourDemold
Pot Life 45.0 - 60.0 min45.0 - 60.0 min
 
Descriptive Properties
ColorBright White
Freeze/Thaw Resistance300 cycles
Mix Ratio100 Parts Gypsum + 50 Parts C-1 Latex + 10 Parts C-2 Resin + 0.5 Parts C-3 Hardener
Specific Volume17.45[in3/lb]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN319 / 297020

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.