MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sharadaa Ceramics Sharada RFC-45 Gel Bonded Castables
Categories: Ceramic

Material Notes: Mullite Bonded Free Flowing Cement Free Versatile Castable System

Product Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, Extreme resistance to thermal, Ultra high creep resistance-High HMOR, Intricate shaped Precast blocks superior to fired and Resistance to Mill scale /Accretion

Industry Focus: Steel: Blast Furnace Trough, Torpedo Ladles, Lances/Snorkel, Burner Blocks, Reheat furnace roof/Hearth, Coke Oven door/Roof Repair, Sponge Iron DRI Maintenance, Tundish Flow control device/Well blocks/Nozzles; Cement: Burner Pipe; Non Ferrous: Non wetting to Aluminum/Copper, Lined in Melting furnace walls, Launders, Aluminum Transfer Ladles; Ceramic: Fused silica kiln furniture for Ultra Low thermal, Expansion and High resistance to thermal shock; Ferrous Foundry: Ladles; Glass: Repair of Silica Roof, Sub paving.

Information provided by Sharadaa Ceramics Pvt. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density  2.10 g/cc
@Temperature 1400 °C
0.0759 lb/in³
@Temperature 2550 °F
 2.20 g/cc
@Temperature 800 °C
0.0795 lb/in³
@Temperature 1470 °F
 2.30 g/cc
@Temperature 200 °C
0.0831 lb/in³
@Temperature 392 °F
Porosity 17 %17 %
 18 %18 %
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.0800 GPa
@Temperature 1400 °C
11.6 ksi
@Temperature 2550 °F
Hot
Compressive Strength  34.3 MPa
@Temperature 800 °C
4980 psi
@Temperature 1470 °F
Cold Crushing
 49.0 MPa
@Temperature 1400 °C
7110 psi
@Temperature 2550 °F
Cold Crushing
 
Component Elements PropertiesMetricEnglishComments
Al2O3 45 %45 %
Fe2O3 1.0 %1.0 %
 
Descriptive Properties
Base MaterialMolochite
Permanent Linear Change-1.0 - 1.0%1400°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1045 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
Sinotek Materials WT90-45/75 Amorphous Graphite Powder
Sharadaa Ceramics HH 45 Normal Medium and High Heat and Super Duty Brick
AISI 1045 Steel, turned, ground, and polished, 19-32 mm (0.75-1.25 in) round
AISI 1045 Steel, cold drawn, low temperature, stress relieved round (16 - 22 mm)

CSHARA053 / 130216

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.