System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Polyram PlusTek PA840G3 Nylon 6.6, 15% Glass Fiber
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, 20% Glass Fiber Filled
Material Notes:
15% glass fiber reinforced, impact modified polyamide 6.6 for injection molding applications
Information provided by Polyram Ram On Ind.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.22
g/cc
DIN 53479
Water Absorption
6.5 %
DIN 53495
Moisture Absorption at Equilibrium
2.0 %
50%RH; DIN 53714
Linear Mold Shrinkage
0.00
-
0.0040
cm/cm
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
121
ASTM-D785
Tensile Strength, Yield
110
MPa
ASTM-D638
Elongation at Break
3.5 %
ASTM-D638
Flexural Strength
180
MPa
ASTM D790
Flexural Modulus
4.50
GPa
ASTM-D790
Izod Impact, Notched
1.00
J/cm
@Temperature 23.0 °C
ASTM-D256
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+15
ohm-cm
DIN 53482
Surface Resistance
1.00e+12
ohm
DIN 53482
Dielectric Constant
3.5
@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength
90.0
kV/mm
VDE 0303/4
Thermal Properties
Original Value
Comments
Melting Point
256
°C
Maximum Service Temperature, Air
110
°C
Continuous Use
230
°C
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi)
250
°C
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi)
230
°C
DIN 53461
Flammability, UL94
HB
@Thickness 3.00 mm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Lehmann & Voss LUVOCOM® 1-8181 Polyamide 66 with carbon fiber, toughness-modified
Azoty Tarnow™ Tarnamid® T-27 GF10 MX10 Polyamide 6 - Flame Retarded, Reinforced
Azoty Tarnow™ Tarnamid® T-27 GF15 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Eurotec® Tecomid® NA40 GR13 NL100 MB PA6.6, 13% glass fiber reinforced, impact modified, heat stabilized, natural
Eurotec® Tecomid® NA40 GR14 NL MC PA6.6, 14% glass fiber reinforced, impact modified, heat stabilized, natural
PPOLYRA251 / 57513
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.