MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® M901 Epoxy Resin Matrix
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: HexPly® M901 is a hotmelt, thermosetting, high-tack epoxy resin matrix, suitable for prepreg applications at which cure cycles of 130°C and above are required. HexPly® M901 is specifically designed for manufacture of structural composites that are exposed to harsh thermal and environmental conditions. Upon cure within the recommended temperature range of 130 – 170°C, HexPly® M901 exhibits a high glass transition point and an excellent retention of its physical properties after hot-wet treatment. Short cure cycles of 10min and below can be applied to obtain an excellent green strength of the composite part, ready for demolding and further processing. A maximum glass transition point of 195°C can be obtained by postcure of the matrix at elevated temperatures. The product has an excellent shelf life, achieving 15 weeks at ambient conditions and 3 weeks at 35°C.

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 - 1.25 g/cc0.0397 - 0.0452 lb/in³ISO1183-1
Viscosity  600 cP
@Temperature 120 °C
600 cP
@Temperature 248 °F
@ 5°C/min
 1.00e+7 cP
@Temperature 30.0 °C
1.00e+7 cP
@Temperature 86.0 °F
@ 5°C/min
 1.00e+8 cP
@Temperature 141 °C
1.00e+8 cP
@Temperature 286 °F
@ 5°C/min
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg >= 136 °C>= 277 °FHot-Wet
 >= 193 °C>= 379 °FDry
 
Processing PropertiesMetricEnglishComments
Cure Time  5.00 min
@Temperature 160 °C
0.0833 hour
@Temperature 320 °F
Typical Cured Tg (+/-5°C): 180°C
 7.00 min
@Temperature 150 °C
0.117 hour
@Temperature 302 °F
Typical Cured Tg (+/-5°C): 170°C
 10.0 min
@Temperature 130 °C
0.167 hour
@Temperature 266 °F
Typical Cured Tg (+/-5°C): 160°C
 10.0 min
@Temperature 140 °C
0.167 hour
@Temperature 284 °F
Typical Cured Tg (+/-5°C): 175°C
Shelf Life  0.750 Month
@Temperature 35.0 °C
0.750 Month
@Temperature 95.0 °F
 3.75 Month
@Temperature 23.0 °C
3.75 Month
@Temperature 73.4 °F
 >= 6.00 Month
@Temperature 5.00 °C
>= 6.00 Month
@Temperature 41.0 °F
 18.0 Month
@Temperature -18.0 °C
18.0 Month
@Temperature -0.400 °F
 
Descriptive Properties
ColorOff-White/Yellowish

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9178 / 322334

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.