MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
302 Stainless Steel, 25% hardened strip
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Austenitic Cr-Ni stainless steel. More corrosion resistant than Type 301 and because of higher Ni content does not work harden as quickly as Type 301. Essentially non-magnetic in annealed condition, slightly magnetic in cold worked condition. Can be stamped, blanked, formed, and lightly drawn. Applications include car and radar antennas, automobile trim, bottling machinery, dairy processing equipment, food processing equipment, home appliances, hospital equipment, industrial floor plate, jewelry, kitchen and restaurant equipment, spring clips, washers, retainers.

Key Words: T302, T 302, 302SS, 302 SS, UNS S30200, AMS 5515, AMS 5516, AMS 5636, AMS 5637, AMS 5688, ASME SA 240, ASME SA 479, ASTM A167, ASTM A240, ASTM A276, ASTM A313, ASTM A314, ASTM A368, ASTM A473, ASTM A478, ASTM A479, ASTM A492, ASTM A493, ASTM A511, ASTM A554, ASTM A666, FED QQ-S-763, FED QQ-S-766, FED QQ-W-423, MIL SPEC MIL-S-862, SAE J230, SAE J405 (30302), DIN 1.4300, X12CrNi188, B.S. 309S25, EN 58A, PN 86020 (Poland), 1H18N9, austenitic, ISO 4954 X10CrNi189E, ISO 683/13 12, ISO 6931 X9CrNi188, 18-8
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.86 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 261Converted from Rockwell C hardness.
Hardness, Knoop 277Converted from Rockwell C hardness.
Hardness, Rockwell B 98Converted from Brinell
Hardness, Rockwell C >= 25
Hardness, Vickers 269Converted from Rockwell C hardness.
Tensile Strength, Ultimate >= 860 MPa
Tensile Strength, Yield >= 515 MPa
@Strain 0.2 %
Elongation at Break 12 %in 50 mm
Modulus of Elasticity 193 GPa
Poissons Ratio 0.25Calculated
Fatigue Strength 485 - 550 MPaT302 with full hardened temper
Shear Modulus 77.2 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000720 ohm-cm
@Temperature 20.0 °C
 0.0000780 ohm-cm
@Temperature 100 °C
 0.0000860 ohm-cm
@Temperature 200 °C
 0.000100 ohm-cm
@Temperature 400 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.2 µm/m-°C
@Temperature 0.000 - 100 °C
 17.8 µm/m-°C
@Temperature 0.000 - 315 °C
 18.4 µm/m-°C
@Temperature 0.000 - 540 °C
 18.7 µm/m-°C
@Temperature 0.000 - 650 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 16.2 W/m-K
@Temperature 100 °C
 21.5 W/m-K
@Temperature 500 °C
Melting Point 1400 - 1420 °C
Solidus 1400 °C
Liquidus 1420 °C
Maximum Service Temperature, Air 870 °CIntermittent
 925 °CContinuous Service
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.15 %
Chromium, Cr 18 %
Iron, Fe 70 %
Manganese, Mn <= 2.0 %
Nickel, Ni 9.0 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
302 Stainless Steel, annealed strip
304 Stainless Steel
301 Stainless Steel
302 Stainless Steel, annealed bar
302 Stainless Steel, after cold work

MQ302AB / 12622

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.