Multi-Flex® G 7155 is based on Shell's Kraton G technology, manufactured under the license of Shell. Multibase certifies that his product has been formulated with the same ingredients as manufactured by Shell, under the reference Kraton G 7155 and complies to the internal specifications of Shell/Multibase. The burn rate is 0.99 in/min (24.8 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G. Data provided by Multibase. |