MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
3M Nextel™ 610 Composite Ceramic Fiber
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Composite Fibers

Material Notes: Chemical composition above is wt%. Filament diameter is 10-12 µm.

3M Nextel Ceramic Fibers 610, 650, and 720 are composite grade fibers. They have a refined crystal structure based on alpha-Al2O3 and do not contain glassy phases. This allows the fibers to retain their strength at high temperatures. 3M Nextel Fiber 610 is a fine grained single-phase composition of alpha-Al2O3. It has the highest strength at room temperature. However, because it is essentially single phased, the strength decreases rapidly at high temperatures due to grain growth.

Information provided by 3M Ceramic Textile and Composites.

Key Words: Alumina, Aluminum Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.90 g/cc
Particle Size <= 0.50 µmCrystal size
Specific Surface Area <= 0.20 m²/g
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 3100 MPa
@Thickness 25.4 mm
filament
Tensile Modulus 373 GPaFilament property
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.00 µm/m-°C
@Temperature 100 - 1100 °C
Melting Point 2000 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.74
 
Component Elements PropertiesOriginal ValueComments
Al2O3 >= 99 %
 
Descriptive Properties
ColorOff-White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Nextel™ 312 Industrial Ceramic Fiber
3M Nextel™ 550 Industrial Ceramic Fiber
3M Nextel™ 720 Composite Ceramic Fiber
3M Nextel™ 440 Industrial Ceramic Fiber
3M Nextel™ 650 Composite Ceramic Fiber

CMMM03 / 1615

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.