MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman PP 3476 Polypropylene Homopolymer, Fiber Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Fiber Grade

Material Notes: Polypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.905 g/ccASTM D792
Melt Flow 18 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 35.0 MPa50 mm/min; ASTM D638
Elongation at Yield 9.0 %50 mm/min; ASTM D638
Tenacity 2.90 g/denierprocess conditions: draw ratios - 3.3, roll speed - 1250 m/min, spring temp - 225°, D 1000/68; ASTM D2556
Flexural Modulus 190000 psiASTM D790
Izod Impact, Notched 0.500 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 164 °Cby DSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin (European Grade)
Borealis HL504FB Polypropylene Homopolymer
Total 7823MZ Polypropylene, Injection Molding Grade
Total 7235 Polypropylene, Blow Molding Grade
Total 3829 Polypropylene, Injection Molding Grade

PASHU249 / 25213

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.