MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Admex™ 523 Polymeric Plasticizer
Categories: Other Engineering Material

Material Notes: Product Description: Admex™ 523 is a low molecular weight polymeric plasticizer that is characterized by a mild ester odor and light color. It imparts excellent processability to PVC compositions. It also has high gel strength, low fusion temperatures and excellent cell structure.

Application/Uses:

  • Coatings
  • Flexible PVC
  • Polyurethane
  • PVC plastisols

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Viscosity  70 cP
@Temperature 95.0 °C
70 cP
@Temperature 203 °F
 5500 - 6500 cP
@Temperature 25.0 °C
5500 - 6500 cP
@Temperature 77.0 °F
Vapor Pressure <= 1.00e-9 bar<= 7.50e-7 torr
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 3.0<= 3.0
 
Thermal PropertiesMetricEnglishComments
Boiling Point >= 300 °C>= 572 °F
Pour Point -9.00 °C15.8 °F
Flash Point 203 °C397 °FClosed Cup
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.511.51
 
Descriptive Properties
ColorPt-Co

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5012 / 222206

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.