MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution PS 1900 GPPS
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Extrusion Grade

Material Notes: Foam extrusion
  • Very high flow
  • High heat resistance
  • Free of zinc and oil additives

Information provided by Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D 792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D 955
Melt Flow 23 g/10 min
@Load 5.00 kg,
Temperature 200 °C
23 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7474ASTM D 785
Tensile Strength, Yield 34.5 MPa5000 psiASTM D 638
Elongation at Break 1.0 %1.0 %ASTM D 638
Tensile Modulus 2.96 GPa430 ksiASTM D 638
Flexural Strength 68.9 MPa10000 psiASTM D 790
Flexural Modulus 3.31 GPa480 ksiASTM D 790
Izod Impact, Notched 0.160 J/cm0.300 ft-lb/inASTM D 638
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.5
@Thickness 1.00 mm,
Frequency 1e+6 Hz
2.5
@Thickness 0.0394 in,
Frequency 1e+6 Hz
ASTM D 150
Dielectric Strength 19.7 kV/mm500 kV/inASTM D 696
 
Thermal PropertiesMetricEnglishComments
CTE, linear 72.0 µm/m-°C40.0 µin/in-°FASTM D 696
Vicat Softening Point 105 °C
@Load 1.02 kg
221 °F
@Load 2.25 lb
120°C/h; ASTM D 1525
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.59
@Wavelength 589.3 nm
1.59
@Wavelength 589.3 nm
Sodium D Line; ASTM D 542
Transmission, Visible 88 - 90 %
@Wavelength 550 nm
88 - 90 %
@Wavelength 550 nm
ASTM D 1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos Nova 2580 General Purpose Crystal Polystyrene
Ineos Nova 3900 General Purpose Crystal Polystyrene
INEOS Styrolution PS 3100/3101 GPPS
Total PSC 1960N Crystal Polystyrene
INEOS Styrolution PS 158K GPPS

PBASG1072 / 159615

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.