MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M F-9752PC Adhesive Transfer Tapes with 420 Adhesive
Categories: Polymer; Adhesive

Material Notes: 2.0 mil, 420 high tack acrylic adhesive with 4.2 mil, 58 lb polycoated kraft paper liner.

Features:

  • 2.0 mil adhesive transfer tape. 58 lb polycoated kraft paper liner. 420 Acrylic Adhesive
  • High tack adhesive. Can be applied in temperatures as low as 32 degrees Fahrenheit
  • Bonds gaskets and foams. Bonds polycarbonate instrument panels.
  • General Industrial Applications, Automotive, Transportation
  • This is good for adhering, joining, affixing, bonding, mounting, holding, and attaching dissimilar materials. Plastic film lamination bonding, splicing, foam laminating, Gasket and foam attachment

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 milTape Only
 102 microns4.00 milRelease Liner
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.438 kN/m2.50 plito Steel; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °FLong term
 323 °C613 °FShort term
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Adhesive Type420
AppearanceClear
LinerMoisture Resistant Tan Paper

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM33253 / 168000

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.