Data provided by the manufacturer, ComAlloy International Company. 30% Glass Fiber/Bead Reinforced. The ComAlloy product line has been integrated into the A Schulman product line. |
Polyamide 6; ComAlloy International Company, subsidiary of A. Shulman Inc. |