MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company ESD 3485-3 Liquid Crystal Polymer (LCP), Carbon Fiber - Electrically Conductive - EMI/RFI/ESD Protection
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Carbon Fiber Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.48 g/ccASTM D 792
Additive Loading 30 %Primary Additive
Linear Mold Shrinkage 0.00 - 0.00020 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 22000 psiASTM D 638
Elongation at Break 1.0 %ASTM D 638
Tensile Modulus 5000 ksiASTM D 638
Flexural Strength 33500 psiASTM D 790
Flexural Modulus 3500 ksiASTM D 790
Izod Impact, Notched 1.30 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 7.00 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 100 ohm-cmASTM D 257
Surface Resistance <= 10000 ohmESD STM11.11
Surface Resistivity per Square <= 1e+05ASTM D 257; ESD STM11.11
Static Decay <= 0.50 secFTMS101C; 4046.1
Shielding Effectiveness 40 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
ASTM D 4935
 40 dB
@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
ASTM D 4935
 40 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
ASTM D 4935
 41 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
ASTM D 4935
 42 dB
@Thickness 2.00 mm,
Frequency 1.50e+8 Hz
ASTM D 4935
 43 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
ASTM D 4935
 43 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
ASTM D 4935
 45 dB
@Thickness 2.00 mm,
Frequency 3.00e+7 Hz
ASTM D 4935
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 545 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 630 - 690 °F
Mold Temperature 150 - 250 °F
Drying Temperature 300 °F
@Time 28800 sec
Dew Point -20.0 °F
Injection Pressure 12000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PQZPA45727 / 279731

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.