MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ineos K44-06-123 Extrusion Grade Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: A black high density polyethylene copolymer specifically for extrusion of potable water, industrial, and mining pipe. It has NSF certification and is recognized by the Plastic Pipe Institute as having a PE 3408 rating. The natural version of this resin is K44-06-122.

Notch Tensile (PENT) is > 100 hrs. per ASTM F 1473. Carbon black loading is 2.3% per ASTM D 1603. Cell classification is 345464C per ASTM D 3350. Hydrostatic design basis is 11.0 MPa (1600 psi) at 23°C and 6.9 MPa (1000 psi) at 60°C per ASTM D 2837.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.944 g/ccASTM D4883
 0.955 g/ccBlack Density
Environmental Stress Crack Resistance >= 5000 hourCondition C; ASTM D1693
Melt Flow 6.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 66ASTM D2240
Tensile Strength, Ultimate 31.0 MPa2 in/min; ASTM D638
Tensile Strength, Yield 22.8 MPa2 in/min; ASTM D638
Elongation at Break >= 800 %2 in/min.; ASTM D638
Flexural Modulus 0.827 GPa
@Strain 2 %
Method 1; ASTM D790
Izod Impact, Notched 3.20 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 126 °CASTM D1525
Brittleness Temperature <= -118 °CASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NOVA Chemicals Sclair® SD-7250-0B HDPE Extrusion Resin
Overview of materials for High Density Polyethylene (HDPE), Extruded
NOVA Chemicals Novapol® HE-Y449-AC HDPE Extrusion Resin
LyondellBasell Petrothene® LR734045 High Density Polyethylene (Sheet & Profile Extrusion)
LyondellBasell Petrothene® LR734011 High Density Polyethylene (Sheet & Profile Extrusion)

PSOLKG / 68224

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.