MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials RTV112 One Component Acetoxy Adhesive Sealant, White
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. Acetic acid vapors are released from the sealant surface as a by-product of cure.

RTV 112 and 118 sealants are self-leveling products which are preferable to paste-consistency sealants when flow into small crevices and hard to reach places is desired.

Key Performance Properties:

  • One-component products
  • Capability to cure at room temperature and ambient humidity
  • Self adhesion properties
  • Low temperature flexibility
  • High temperature performance
  • Excellent weatherability and ozone and chemical resistance
  • Excellent electrical insulation properties

Applications:

Electrical insulation, thin section potting, self leveling protective coatings. Will flow into small crevices and hard to reach places.

FDA 21 CFR 177.2600 USDA NSF International Std. No. 51

GE Silicones became a part of Momentive Performance Materials in 2006.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/cc
Viscosity 20000 cP
Linear Mold Shrinkage 0.010 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 25
Tensile Strength, Ultimate 23.0 kg(f)/cm²
Elongation at Break 325 %
Adhesive Bond Strength 0.686 MPaAt 100% cohesive failure
Peel Strength 15.0 pliAt 100% cohesive failure using 1 in. x 8 in. stainless steel screen at 180° pull angle
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.00e+14 ohm-cm
Dielectric Constant 2.8
@Frequency 60 Hz
Dielectric Strength 16.0 kV/mm
Dissipation Factor 0.0010
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 270 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 0.000500 cal cm/sec-cm²-°C
Maximum Service Temperature, Air 204 °CContinuous
 260 °CIntermittent
Brittleness Temperature -60.0 °C
 
Processing PropertiesOriginal ValueComments
Tack-Free Time 0.333 hour
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
USDA Yes
 
Descriptive Properties
ColorWhite
ConsistencySelf-leveling

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
Henkel Loctite® Durabond® E-30CL Epoxy Adhesive
Momentive Performance Materials RTV142 White, Low Volatile, One Component Silicone Sealant
Dow 732 MULTI-PURPOSE SEALANT
Aluminum 2024-T6

PGESIL012 / 41003

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.