MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Cast 3113 General Purpose Epoxy Casting Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-CAST 3113 is a low viscosity two-part formulation recommended for general purpose electrical potting and encapsulating applications where the combination of good mechanical thermal and electrical properties are required. It is an all liquid system with excellent flow and wetting characteristics, exhibits superior adhesion to glass, ceramics, most metals, many plastics (including potting shells), and other electronics. materials, contains no solvents, and is easily mixed, handled and cured with minimum shrinkage at room temperatures. The fully cured TRA-CAST 3113 is an electrical insulator with good impact and thermal shock resistance. It is further resistant to water, weather, gases, galvanic action, petroleum fuels and solvents, alcohol, salts and many acids and alkalis.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.58 g/ccMixed
Solids Content 100 %Reactive Solids Content
Viscosity 4000 cP
@Temperature 25.0 °C
Mixed (10 rpm)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+16 ohm-cm
 4.00e+14 ohm-cm
@Temperature 100 °C
Dielectric Constant 3.8
@Frequency 100000 Hz
 4.1
@Frequency 1000 Hz
Dielectric Strength 510 V/mil
Dissipation Factor 0.010
@Frequency 1000 Hz
 0.010
@Frequency 100000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 35.0 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 145 °C
Minimum Service Temperature, Air -60.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 hour
@Temperature 65.0 °C
 24.0 hour
@Temperature 25.0 °C
Pot Life 30 min
 
Descriptive Properties
Color Blue
Heat Distortion Temperature °C102
Mix Ratio, parts by weight100/105Resin/Hardener
Thixotropic Index 1.35 rpm/50 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aptek 6106-A/B Epoxy Encapsulant and/or Potting Compound
BCC Products BC 9060 Silicone RTV Rubber
Abatron 75073 A/B Filled Potting Compound
Aptek 6110-A/B Epoxy Encapsulant and/or Potting Compound
Tra-Con Tra-Cast 3145 Thermally Conductive Electrically Insulating Compound

PTRAC107 / 71035

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.