MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Bostik Flex-A-Lastic® Acrylic Mortar
Categories: Other Engineering Material

Material Notes: Description: Bostik Flex-A-LasticR Admixture is a premium grade, high solids acrylic mortar admixture. When mixed with Bostik Tile-MateR Thin Set Mortars, it becomes a flexible, high strength, freeze/ thaw resistant mortar system for the interior and exterior setting of ceramic tile, porcelain tile, marble, granite and large dimension stone. Flex-A-Lastic is an ideal choice for installations requiring high bond strength and flexibility over conventional and unconventional substrates. It also provides tenacious grab making it ideal for vertical applications.

Information provided by Bostik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 546 psi
Flexural Strength 1175 psi
Shear Strength 150 psiQuarry tile; ANSI 118.4
 200 psiPorcelain; ANSI 118.4
 300 psiGlazed wall tile; ANSI 118.4
 450 psiQuarry tile, Flex-A-Lastic
 600 psiPorcelain, Flex-A-Lastic
 658 psiGlazed wall tile, Flex-A-Lastic
 
Processing PropertiesOriginal ValueComments
Cure Time 18.0 hourFinal Set
Shelf Life 12.0 Month
@Temperature 1.11 - 37.8 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBOSTK017 / 191553

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.