MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Molybdenum Mo-0.5Ti; M0-0.5Ti-0.02C (Molybdenum Alloy 362)
Categories: Metal; Nonferrous Metal; Molybdenum Alloy; Refractory Metal

Key Words: UNS R03620, Specifications: ASTM B384, ASTM B385, ASTM B386, ASTM B387
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 10.2 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 76.0 MPa
@Temperature 1650 °C
 415 MPa
@Temperature 1095 °C
 895 MPa
@Temperature 23.0 °C
Tensile Strength, Yield 48.0 MPa
@Temperature 1650 °C
 345 MPa
@Temperature 1095 °C
 825 MPa
@Temperature 23.0 °C
Elongation at Break 10 %
Tensile Modulus 315 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.10 µm/m-°C
@Temperature 20.0 - 1010 °C
Specific Heat Capacity 0.250 J/g-°CEstimated from Pure Mo.
Thermal Conductivity 125 W/m-KEstimated from Pure Mo.
Melting Point <= 2610 °C
Liquidus 2610 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.010 - 0.040 %
Iron, Fe <= 0.010 %
Molybdenum, Mo 99.5 %
Nickel, Ni <= 0.0050 %
Nitrogen, N <= 0.0010 %
Oxygen, O <= 0.0030 %
Silicon, Si <= 0.010 %
Titanium, Ti 0.40 - 0.55 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Molybdenum, Mo, Annealed
Molybdenum TZC (Mo-1Ti-0.3Zr)
Overview of materials for Molybdenum Alloy
CuMoCu 13/74/13
W-50Mo Tungsten Alloy

MRMo00 / 13889

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.