Availability: North America Forms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 33% Filler by Weight Additive: Lubricated Features: Lubricated Processing Method: Injection Molding Appearance: Black Information provided by TP Composites, Inc. |