MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Baytec® MS-051 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Baytec MS-051 is a modified diphenylmethane diisocyanate (MDI)-terminated polyester prepolymer.

Properties / Applications: Baytec MS-051 is a modified diphenylmethane diisocyanate (MDI)-terminated polyester prepolymer used in the manufacture of high-property solid cast polyurethane elastomers. The excellent resilience and low compression-set properties have enabled this material to be used for low-durometer wheels, printing rolls, and squeegee blades. As with any product, use of Baytec MS-051 prepolymer in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/cc
@Temperature 100 °C
 1.18 g/cc
@Temperature 80.0 °C
Viscosity 700 cP
@Temperature 100 °C
 2700 cP
@Temperature 80.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80BDO; ASTM D2240
 93HQEE; ASTM D2240
Tensile Strength at Break 26.3 MPaHQEE; ASTM D412
 37.0 MPaBDO; ASTM D412
 4.41 MPa
@Thickness 2540 mm
BDO; ASTM D412
 6.00 MPa
@Thickness 5080 mm
BDO; ASTM D412
 8.07 MPa
@Thickness 2540 mm
HQEE; ASTM D412
 8.14 MPa
@Thickness 7620 mm
BDO; ASTM D412
 9.89 MPa
@Thickness 5080 mm
HQEE; ASTM D412
 11.8 MPa
@Thickness 7620 mm
HQEE; ASTM D412
Elongation at Break 525 %BDO; ASTM D412
 650 %HQEE; ASTM D412
Compressive Strength 0.241 MPa
@Strain 2 %
BDO; ASTM D575
 0.621 MPa
@Strain 2 %
HQEE; ASTM D575
 0.724 MPa
@Strain 5.0 %
BDO; ASTM D575
 1.52 MPa
@Strain 10 %
BDO; ASTM D575
 1.69 MPa
@Strain 5.0 %
HQEE; ASTM D575
 2.28 MPa
@Strain 15 %
BDO; ASTM D575
 2.90 MPa
@Strain 10 %
HQEE; ASTM D575
 3.07 MPa
@Strain 20 %
BDO; ASTM D575
 3.93 MPa
@Strain 25 %
BDO; ASTM D575
 3.96 MPa
@Strain 15 %
HQEE; ASTM D575
 5.03 MPa
@Strain 20 %
HQEE; ASTM D575
 6.21 MPa
@Strain 25 %
HQEE; ASTM D575
 10.9 MPa
@Strain 50 %
BDO; ASTM D575
 18.4 MPa
@Strain 50 %
HQEE; ASTM D575
Resilience 52Bayshore, BDO; ASTM D2632
 54Bayshore, HQEE; ASTM D2632
Tear Strength 105 pliSplit, BDO; ASTM D1938
 280 pliSplit, HQEE; ASTM D1938
 380 pliDie C, BDO; ASTM D624
 615 pliDie C, HQEE; ASTM D624
Taber Abrasion, mg/1000 Cycles 16
@Load 1.00 kg
H-18, BDO; ASTM D4060
 34
@Load 1.00 kg
H-18, HQEE; ASTM D4060
Compression Set 19 %
@Temperature 70.0 °C,
Time 79200 sec
HQEE; ASTM D395-B
 24 %
@Temperature 70.0 °C,
Time 79200 sec
BDO; ASTM D395-B
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 93.0 °C
 
Processing PropertiesOriginal ValueComments
Mold Temperature 100 - 110 °C
 
Descriptive Properties
AppearanceLight amber liquid
Content4.9-5.2%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sorbothane Polyurethane Damping Material, 50 Durometer
Daikin DAI-EL® G-101 Fluoroelastomer Plasticizer with DAI-EL® G-701 Fluoroelastomer
SMAC SMACTANE® SP Damping Material
SMAC SMACTANE® 50 1114S- N03 Damping Material
Shin-Etsu Silicones SF-11500U Fluorosilicone Elastomer

PCOVEST0253 / 202036

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.