MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Huntsman IROGRAN® A 92 E 5670 FCM Ester-Based TPU-For Food Contact
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Introduction: IROGRAN A 92 E 5670 FCM is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion/injection molding product range and offers a specially designed, flexible material with a broad processing window. IROGRAN A 92 E 5670 FCM is a food contact material.

Performance Features:

  • High oil resistance
  • High production rate
  • Good melt flow
  • Easy coloring
  • Complies with FDA CFR 175.105 / 177.2600
Applications:
  • Cable jacketing
  • Tubing
  • Technical extrusion

Information provided by Huntsman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASDTM D792
Linear Mold Shrinkage 0.0040 cm/cmASTM D955
Melt Index of Compound 62 g/10 min
@Load 10.0 kg,
Temperature 190 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90ASTM D2240
Hardness, Shore D 38ASTM D2240
Tensile Strength at Break 40.0 MPaDIN 53504
Elongation at Break 570 %DIN 53504
Compression Set 25 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D395
 40 %
@Temperature 70.0 °C,
Time 86400 sec
ASTM D395
 
Processing PropertiesOriginal ValueComments
Feed Temperature 195 °C
Front Barrel Temperature 205 °C
Adapter Temperature 210 °C
Die Temperature 210 °C
Roll Temperature 170 - 190 °CFront, 32 rpm
 170 - 190 °CRear, 27 rpm
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips HiD® 99413F with Food Grade Antistat HDPE Blow Molding Resin
Huntsman IROGRAN® A 85 P 4394 FCM Ether-Based TPU-For Food Contact
Petromont 3101 High Density Polyethylene Resin
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether
Huntsman IROGRAN® A 85 P 4441 FCM Ether-Based TPU-For Food Contact

PHU9940 / 150400

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.