MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Empilon EMPILON® 665T TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: EMPILON® 6 series products own high transparency, high elasticity, good physical and mechanical properties, and medical food requirements. They are often used in medical, food, and shock-absorbing materials and have high transparency; it is a blending material mainly based on hydrogenated Styrenic Block Copolymer. The hardness ranges from Shore OO33 to Shore A80. It can be processed by injection molding, extrusion molding and calendaring. The series is non-toxic. It does not contain RCRA 8 heavy metals, halogens, phthalate and is 100% recyclable and eco-friendly. It can pass the European Union Waste Electronics and Electrical Equipment (WEEE), Restriction of Hazardous Substances (RoHS) regulations and meet the environmental requirements of SONY SS-00259 4th Edition. This series owns excellent mechanical property, weather and heat resistance, good resilience and has low specific gravity, good chemical resistant and hydrolysis resistant performance. This series can be used without drying before processing. If you want to dye this series of products, please choose PE or EVA as the substrate of masterbatch, never use PVC as the substrate. Moreover, use a higher screw speed when processing and higher back pressure to achieve better dispersion of the colorant.

Series Features:

  • Excellent Heat Aging Resistance
  • Low Specific Gravity
  • Excellent Mechanical Property and Toughness
  • High Transparency
  • Excellent Resilience
  • Extremely Low Hardness
  • Apply to high toughness, high elastic recover demand product
  • Apply to high transparent elastic product
  • Apply to medical food grade products
  • Injection molding, extrusion molding, calendaring and other processing technology
Applications:
  • Syringe Plug: Medical Regulation/Sealing Performance
  • Icebox: Food Safety/Low Temperature Resistance
  • Braces: Transparency/High Toughness
  • Sex Toys: Medical Regulations/Resilience
  • Medical Equipment: Medical Regulations
  • Snorkel: Transparency/Resilience

Information provided by EMILON®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.890 g/cc0.890 g/ccASTM D792
Melt Flow >= 35 g/10 min
@Load 5.00 kg,
Temperature 190 °C
>= 35 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 72
@Time 10.0 sec
72
@Time 0.00278 hour
ASTM D2240
Tensile Strength 4.90 MPa711 psiASTM D412
Elongation at Break 460 %460 %ASTM D412
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -50.0 °C-58.0 °F
Shrinkage, MD 1.0 %1.0 %
Shrinkage, TD 1.3 %1.3 %
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 70 %70 %HT Method
 
Processing PropertiesMetricEnglishComments
Feed Temperature 165 - 175 °C329 - 347 °F
Middle Barrel Temperature 175 - 190 °C347 - 374 °F
Front Barrel Temperature 185 - 195 °C365 - 383 °F
Nozzle Temperature 185 - 200 °C365 - 392 °F
Melt Temperature 165 - 200 °C329 - 392 °F
 <= 230 °C<= 446 °Fdo not exceed
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Injection Pressure 3.43 - 4.90 MPa497 - 711 psi
Back Pressure 0.490 - 0.785 MPa71.1 - 114 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEMPIL021 / 294708

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.