MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zircar Refractory Composites RS-201 Refractory Sheet
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: ZRCI Refractory Sheet Type RS-201 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivity and excellent electrical insulation. It retains strength and utility to levels far exceeding maximum use temperatures of reinforced plastics and asbestos cement replacements. It is 100% inorganic, non-flammable and contains no asbestos. Its high alumina content makes it resistant to many environments including molten aluminum. RS-201 undergoes little or no outgassing on heating, is not brittle, and may be cut and machined with standard tooling. RS-201 has a highly burnished outside surface. This is ideal when the OD is crucial for liner placement. It is available in standard and custom size cylinders and are useful as induction coil liners, induction furnace components, and molten metal transport tubes.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.08 g/cc
Porosity 30 %
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.0689 GPa
 0.0207 GPa
@Temperature 1010 °C,
Time 86400 sec
 0.0310 GPa
@Temperature 510 °C,
Time 86400 sec
Compressive Strength 55.1 MPa24 hrs at 510°C, parallel to thickness
 68.9 MPa24 hrs at 1010°C, parallel to thickness
 89.6 MPaparallel to thickness
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.70e+12 ohm-cmASTM D257
Surface Resistance >= 1.30e+13 ohmASTM D257
Dielectric Strength 26.0 V/milASTM D149
Arc Resistance >= 420 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.00 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 4.30 W/m-K
@Temperature 204 °C
parallel to thickness
 4.50 W/m-K
@Temperature 427 °C
parallel to thickness
 4.60 W/m-K
@Temperature 649 °C
parallel to thickness
 4.70 W/m-K
@Temperature 1010 °C
parallel to thickness
Melting Point 1500 °C
Maximum Service Temperature, Air 1260 °C
Shrinkage <= 1.0 %
@Temperature 1010 °C,
Time 86400 sec
perpendicular to thickness
 
Component Elements PropertiesOriginal ValueComments
Al2O3 65 %
B2O3 4.0 %
CaO 8.0 %
MgO 1.0 %
Other 1.0 %
SiO2 21 %
 
Descriptive Properties
ColorWhite to buff

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zircar Refractory Composites RSLE-57 Refractory Sheet
Zircar Refractory Composites RS-200 Refractory Sheet
Crystex Composites Mykroy/Mycalex MM 1301 Molding Grade Glass-bonded Mica Composite
Thermal Transfer Composites PRIMEX Cast™ MCX-1405™ Aluminum Silicon Carbide Composite, Reinforced
Zircar Refractory Composites Alumina Coat

CZRCI17 / 2880

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.