MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
IIMAK METALLOGRAPH™ Conductive Thermal Transfer Ribbon
Material Notes: An aluminum base thermal transfer ribbon (TTR), this product is available for just about any thermal transfer printer on the market. This digital process is excellent for rapid prototyping, design verification and production runs. With no messy clean-up and low capital expenditure, this process is very efficient. Excellent resistivity and processing ease make this an excellent printing solution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
Filler Content 100 %
Thickness 0.250 - 0.270 microns
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.0000030 - 0.0000035 ohm-cm
Surface Resistivity per Square 0.039 - 0.042 ohm
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 0.00 %
 
Descriptive Properties
Adhesion5
Binder SystemNA
Conductive Filler TypeOther
Material TypeReady-To-Use Formulation
Solvent SystemNA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite RX® 2-501N Diallyl Phthalate Compound
Materion C118 Electrical Contact Alloy
Lucas-Milhaupt EASY FLO 30 Silver Based Cadmium-Bearing Filler Metal
LATI Laticonther 62 GR/50 PA 6, 50% Graphite Reinforced
Envalior Stanyl® TC153 PA46 FR(17)

PFLEXCM04 / 179406

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.