MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Borealis RA7050-LG Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: RA7050-LG is a low melt flow rate, light grey in color, PP-RCT (Polypropylene-Random Crystallinity Temperature) material. RA7050-LG has a special crystallinity brought by a special beta-nucleation that exhibits an improved pressure resistance, especially at elevated temperatures. The product data sheet does not release customers from their liability to check that delivered material is fit for purpose and application. RA7050-LG is ready compounded for maximum quality control. The color of RA7050-LG is light grey similar (but not equivalent) to RAL 7032.

Applications: RA7050-LG is in general intended to be used in applications for plumbing and heating, such as in-house hot and cold water pipes and fittings, floor and wall heating systems and radiator connections. The product data sheet does not release customers from their liability to check that delivered material is fit for purpose and application.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 0.250 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
Antiblock Level 1800 ppm
Slip Level 1500 ppm
Storage Temperature <= 50.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 25.0 MPaISO 527-2
Elongation at Yield 10.0 %ISO 527-2
Tensile Modulus 850 MPaISO 527-2
Charpy Impact, Notched 4.00 kJ/m²
@Temperature 0.000 °C
ISO 179-1
 40.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1
 
Processing PropertiesOriginal ValueComments
Processing Temperature 215 - 230 °Ccylinder
 220 - 230 °Ctool
Die Temperature 220 - 230 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9902 / 323259

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.