MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Huber Martoxid® MRS Calcined Aluminum Oxide
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Martoxid® MRS calcined aluminum oxide is an unground aluminum oxide for ceramics with a high Al2O3-content, subjected to extremely high mechanical, thermal, chemical and electrical loads for applications like high efficiency spark plugs and substrates.

CAS No.: 1344-28-1

EC/EINECS No.: 215-691-6

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.900 g/cc0.0325 lb/in³
Particle Size <= 45 µm<= 45 µm0-20 percent, Screening
 45 - 63 µm45 - 63 µm1-15 percent, Screening
 63 - 106 µm63 - 106 µm35-60 percent, Screening
 >= 106 µm>= 106 µm20-50 percent, Screening
Specific Surface Area 1.5 - 2.5 m²/g1.5 - 2.5 m²/gBET
 
Component Elements PropertiesMetricEnglishComments
Al2O3 >= 95 %>= 95 %a-Al2O3
CaO 0.010 %0.010 %
Fe2O3 0.030 %0.030 %
Loss on Ignition(%) <= 0.10 %<= 0.10 %
Na2O <= 0.050 %<= 0.050 %total
SiO2 0.050 %0.050 %
 
Descriptive Properties
Al(OH)3 (%)99.8
FunctionalityInert filler
Market/Application: IndustrialWater Treatment
Primary Crystal1.0-1.4 µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EHUBER819 / 300925

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.