MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotchlite™ 680CR-71 Removable Reflective Graphic Film with Comply™ Adhesive
Categories: Polymer; Film

Material Notes: 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appearance that retains most of this reflectivity when wet; Excellent angularity; Pressure-activated adhesive for easy sliding and tacking; Removable with heat; For vertical, flat, curved or corrugated surfaces, with or without rivets; Air release channels for fast and easy, bubble-free graphic installation

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 178 - 203 microns7.00 - 8.00 milwith adhesive
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.456 kN/m2.60 pliAdhesion to Painted aluminum panels
 0.649 kN/m3.70 pliAdhesion to FRP
 0.841 kN/m4.80 pliAdhesion to Aluminum
 
Processing PropertiesMetricEnglishComments
Processing Temperature 4.00 - 38.0 °C39.2 - 100 °FApplication Temp; flat surfaces without rivets
 7.00 - 38.0 °C44.6 - 100 °FApplication Temp; flat, curved or corrugated surfaces with rivets
 
Descriptive Properties
LinerYellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35106 / 169853

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.