MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Struktol ZINC STEARATE
Categories: Ceramic; Other Engineering Material; Additive/Filler for Polymer

Material Notes:

STRUKTOL® Zinc Stearate is one of the most widely used additives in the plastics field. It serves primarily as a lubricant, but also as a densifying agent and a partitioning agent. It is used extensively in color concentrates as a dispersion aid. It is used to improve processing of the styrenics and polyesters, and to a lesser extent with the olefins. In rubber applications, it functions as an elastomer processing aid and release agent.

FDA Status: 175.105; 175.300; 176.170; 176.180; 176.200; 177.1460; 177.1900; 177.2410; 177.2600; 178.2010; 178.3910; 182.8994

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Additive Loading <= 0.50 %<= 0.50 %In most plastic applications. Up to 3 parts in rubber
Particle Mesh Size 330 Mesh330 Mesh99% through 325 mesh
Ash 15.5 %15.5 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 117 - 123 °C243 - 253 °F
Dropping Point 117 - 127 °C243 - 261 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 1.0 %<= 1.0 %
 
Descriptive Properties
AppearanceWhite bead or pastille
Free Fatty Acid (%, max)1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSTRUK17 / 69245

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.