MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total PPC 4820WZ Polypropylene, Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: TOTAL Petrochemicals Polypropylene 4820WZ is a nucleated impact copolymer with a Melt Flow index of 35 g/10 min.

TOTAL Polypropylene 4820WZ is characterized by improved stiffness, creep resistance, high impact resistance, excellent antistatic properties and has been formulated to allow faster cycling through early demolding.

Total Polypropylene 4820WZ has been developed specifically for the injection molding of garden furniture, housewares, thin-walled articles and compounding.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.905 g/cc0.905 g/ccASTM D1505
Melt Flow 35 g/10 min35 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 27.0 MPa3920 psiASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Flexural Modulus 1.38 GPa200 ksiASTM D790
Izod Impact, Notched  0.370 J/cm
@Temperature -20.0 °C
0.693 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 0.800 J/cm
@Temperature 23.0 °C
1.50 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Charpy Impact, Notched  0.450 J/cm²
@Temperature -20.0 °C
2.14 ft-lb/in²
@Temperature -4.00 °F
DIN 53453
 0.950 J/cm²
@Temperature 23.0 °C
4.52 ft-lb/in²
@Temperature 73.4 °F
DIN 53453
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 - 165 °C320 - 329 °FTOTAL Method
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FPressure unspecified; ASTM D648
Vicat Softening Point 150 °C302 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® 2458 Polycarbonate, Injection Grade
Phillips 66 COPYLENE® CM350LN Polypropylene, Impact Copolymer, Medium Impact, Nucleated, Antistat, Injection Molding
SCG Chemicals EL-Pro™ P842J Polypropylene Injection Molding
Total PPR 3221 Random Copolymer Polypropylene, Blow Molding and Sheet Extrusion
Ineos 3950 Polypropylene Impact Copolymer

PTOTAL870 / 130595

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.