MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CMT Materials HYTAC® C1R Highly Durable Syntactic Foam, Dust-Free Machining/Polishing
Categories: Polymer; Thermoset; Epoxy

Material Notes: HYTAC-C1R is easily machined without the dust typically associated with epoxy syntactic foam. This new copolymer base has been optimized for both the machine shop and the thermoforming process.

Excellent surface characteristics are obtained straight from machining and may be easily modified with sandpaper to carry more or less material into the mold as needed. It may be polished to a very smooth surface when necessary for working with transparent plastics.

HYTAC-C1R has these outstanding attributes:

  • 3 – 4X the toughness of epoxy-based syntactic foam
  • Good machinability
  • Superior edge definition and detail
  • Very low thermal conductivity
  • Excellent material distribution
Variety of Shapes and Sizes: The material is provided in standard sized rods or sheets, but may be custom molded to meet the specific needs.

Applications: HYTAC-C1R is the first material to combine the durability of a thermoplastic syntactic with the dust free, easy machining and polishing capability of a copolymer syntactic foam. Excellent surface characteristics optimize material distribution with most plastics.

Recommended for use with APET, CPET, HIPS, PETG, PLA, PP, PVC and RPET.

Information Provided by CMT Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 46.0 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Flexural Toughness 11.3 psiASTM D790
Compressive Strength 6960 psi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 35.0 µin/in-°F
Thermal Conductivity 0.130 W/m-K
Maximum Service Temperature, Air 350 °F
 
Descriptive Properties
ColorSlate Blue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CMT Materials METAPOR® BF 100 AL Air Permeable Material
CMT Materials HYTAC® FLX Good Durability, Easily Machined & Polished Copolymer Syntactic
SEKISUI SPI KYDEX® 410 ABS/PVC
SEKISUI SPI KYDEX® 430 ABS/PVC
SEKISUI SPI KYDEX® T-LW Thermoplastic

PCMT006 / 146231

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.