MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos Nova 464 High Impact Polystyrene Injection Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Easy flow, Wide processing window

Applications: General purpose moldings

This grade complies with European, German, and US food standards.

Properties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.

Information provided by NOVA Chemicals.

INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 

Key Words: HIPS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO 1183A
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
Melt Flow 18 g/10 minCondition G; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 26.0 MPaISO 527B
Tensile Strength, Yield 28.0 MPaISO 527B
Elongation at Break 40 %ISO 527B
Flexural Modulus 2.40 GPaISO 178
Izod Impact, Notched 1.00 J/cm
@Diameter 3.17 mm
bar, 0.010" notch radius; ISO 180
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °CISO 75
Vicat Softening Point 86.0 °CISO 306A
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Melt Temperature 190 - 274 °C
Mold Temperature 10.0 - 60.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical ALPHALAC SF510 HIPS
Ineos Nova 2114 High Impact Polystyrene Extrusion Grade
A. Schulman Lucent 66-01 Nylon 66, General Purpose, Injection Grade
A. Schulman Lucent 6-01 Nylon 6, General Purpose, Injection Grade
Ascend Performance Materials Vydyne® 842A NT0733 Nylon 66, Extrusion Grade

PNOVA284 / 55185

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.